Boriding of the Ti-Al intermetallic GE48-2-2 at 1273 K for 10 hours was performed. In order to ensure that no any serious alteration occurred in the substrate,
The phase transformation of hydroxyapatite (HAP, Ca10(PO4)6(OH)2) to the beta tricalcium phosphate phase (β-TCP, β-Ca3(PO4)2) at 1100°C is well known. Ho
In this technical paper, the oxidation mechanism and kinetics of aluminum powders are discussed in great details. The potential applications of spherical alumin
In this paper, commercial lithium ion battery cells consisting of graphite based anode and LiNi0.80Co0.15Al0.05O2 (NCA) oxide based cathode were investigated re