论文部分内容阅读
根据55m~3高炉试验的取样数据,岩相鉴定和多孔管试验结果,全面地总结了包钢烧结矿和球团矿在高炉冶炼过程中的行为及破损机理,从而对改善原料的冶金性能提出具体措施。
According to the sampling data, lithofacies identification and multi-hole tube test results of 55m ~ 3 blast furnace test, the behavior and damage mechanism of Baotou sinter ore and pellet in blast furnace smelting process are summarized, and the metallurgical performance of raw material is improved specific measure.