改进炉底烧结方法,提高烧结质量,是提高品种质量,降低原、燃材料消耗的有效措施之一。我厂于1964年1月31日烧结的11号平炉(300吨倾动式平炉,炉底面积64.4米~2,一对格子砖体积292米~3)炉底,吸取了几年来的经验教训,加强了技术操作,采用了细颗粒镁砂,分层加热,高温搥打的措施,获得了显著的效果。使烧结时间缩短到22点10分钟,烧结
To improve the bottom sintering method and improve the sintering quality is one of the effective measures to improve the quality of varieties and reduce the consumption of raw materials and fuel materials. I plant in January 31, 1964 sintered 11 # open hearth furnace (300 tons tilting type hearth, hearth area 64.4 m ~ 2, a pair of checker brick volume 292 m ~ 3) bottom, drawing on the experience of the past few years, Strengthen the technical operation, the use of fine-grained magnesia, stratified heating, high-temperature thrashing measures, access to significant results. The sintering time is shortened to 22:10, sintering