论文部分内容阅读
在湿法炼铜电解过程中,造成阴极表面粗糙、疏松的根本原因,在于阴极附近电解液中铜离子浓度的贫化。在通常情况下,为
In the wet-process copper electrolysis process, the root cause of the cathode surface roughening and looseness lies in the depletion of copper ion concentration in the electrolyte near the cathode. In normal circumstances,