为充分发挥转炉生产能力,实现三吹二或阶段性三吹三连续作业,第三炼钢厂在提高炉龄方面做了很多工作。首先,选择了最佳炉衬材质,实行均衡炉村,按标准化砌炉,稳定冶炼操作,同时采用渣层保护,投补、喷补及操作中渣补等综合炉体维护办法,并且加强对炉龄工作的科学管理,使炉龄分别达到1366次和1486次。突破了千次大关,为提高转炉的生产能力创造了条件。
In order to give full play to the converter capacity, to achieve three blowing two or three blowing three consecutive operations, the third steel mill to improve furnace age done a lot of work. First of all, the best choice of lining material, the implementation of a balanced stove village, according to the standard building furnace, stable smelting operation, while the use of slag protection, casting, spraying and slag and other operations in the maintenance of integrated furnace maintenance, and strengthen the furnace Scientific management of working age, so that the furnace were 1366 times and 1486 times. Break through the thousand mark, to create the conditions for improving the production capacity of the converter.