In this paper,a large-sized ingot of Mg–9Gd–3Y–1.5Zn–0.5Zr(wt%) alloy with a diameter of 600 mm was successfully prepared by the semi-continuous casting met
Ti–51at%Ni shape memory alloys(SMAs) were successfully produced via a powder metallurgy and microwave sintering technique.The influence of sintering parameters