Large undercoolings up to 395K (0.28TE) are obtained for 15g samples of Ni-32.5%Sn eutectic alloy by superheating the alloy melt to 108-700K above its eutectic temperature and consequently destroying most of the inherent heterogeneous nuclei. The recalcsc