【摘 要】
:
本文在总结生产实践经验的基础上,分析了影响制品精度的主要原因,并提出了提高制品精度的措施。变薄拉深制品的精度主要是指制品壁厚差的大小。经过变薄拉深(以下简称为拉深
论文部分内容阅读
本文在总结生产实践经验的基础上,分析了影响制品精度的主要原因,并提出了提高制品精度的措施。变薄拉深制品的精度主要是指制品壁厚差的大小。经过变薄拉深(以下简称为拉深)后的制品都存在着壁厚差,尤其是经过多次拉深成形的制品就更显得突出。
On the basis of summing up the practical experience of production, this paper analyzes the main reasons that affect the accuracy of products, and puts forward the measures to improve the accuracy of products. The precision of thinning and deep drawing products mainly refers to the difference of product wall thickness. After the thinning (hereinafter referred to as drawing) after the products have poor wall thickness, especially after several deep drawing of the product even more prominent.
其他文献
请下载后查看,本文暂不支持在线获取查看简介。
Please download to view, this article does not support online access to view profile.
本文采用光弹性法,电阻应变法,和金相检查法等多种实验手段,对链板方孔、孔边进行了强度分析,改进了力学简图。提出采用门型刚架来代替轴向拉伸计算简图;选择合理孔型;测得角
The visible and near infrared(NIR)(350-2500 nm)spectra and the MOE of 438 small clear wood samples from Chinese fir,eucalyptus and poplar 72 were measured.Using
一台焊接结构设备的质量优劣,不仅与焊接结构本身的设计方案、焊接工艺和焊接规范有关,而且与焊接体的金属切削加工工艺有着密切的关系。如果金工工艺加工顺序安排不当,会直
本文报导了从五个炉号的高锰钢失效辙叉中取样进行的小能量多冲试验结果。用电镜、金相法研究了断裂过程及断口形貌。用俄歇谱仪法测定了晶界磷的偏聚。在该试验条件下多冲寿
××机前起落架转轴接头,原材料为30CrMnSiNiA,零件净重8.5公斤,是一个重要受力件,结构复杂.如图1.原用万吨水压机压制的白由锻坯经机加而成,锻坯重200公斤,机加工时在1000
大家好!又和大家见面了。这次为大家带来的是我的德国情结之我最喜爱的球员托马斯·希策尔斯佩格。本人是一个铁杆德国球迷,所以喜欢的大多数球员都是德国队的。众所周知德国
测定了不同含铁量的电镀 Ni-Fe 合金的稳态腐蚀电位.用恒电流阳极溶解法测定了不同组合体系的层间电位差曲线,并用“EC”法检测了这些组合体系的耐蚀性。确证三层 Ni-Fe 体系
本文研究了成膜胺在盐酸介质中的缓蚀效率,并和常用的酸洗缓蚀剂——乌洛托品做了对比。通过用失重法、比色法、电化学法等实验手段、结果表明:成膜胺在盐酸介质中缓蚀效率优
据山西稷山县卫生局讯中医研究院农村疾病研究所的同志于去年十二月五日到达稷山,受到当地党政领导的热烈欢迎。他们到县后,没有顾上休息,马上就投入紧张的防治疾病的工作。