The pitch was dried and modified with 1 mass%nickel nitrate and 10 mass% Si powder successively,then carbonized in Ar atmosphere at 900,1 000,1 100,1 200,1 300,and 1 400 ℃,respectively. Effects of carbonization temperature on phase composition and microst