论文部分内容阅读
在具有电致发光(EL)的有机整合染料8-羟基喹啉铝(Alq3)中接以染料罗丹明6G(R6G),用真空热蒸发的方法制备器件,获得了峰值波长575nm的黄色直流薄膜电致发光,从而通过掺杂改变了发光颜色.并在Alq3发光层不同区域插入一掺杂薄层(Alq3:R6G),利用其发光波长与未掺杂部分(Alq3)的不同,以此作为“探测层”,通过对器件光谱及电学特性的测量与分析,探讨了有关发光区域,发光机理,界面对发光影响等基本问题.
The dye Rhodamine 6G (R6G) was dipped into the organic integrated dye 8-hydroxyquinoline aluminum (Alq3) with electroluminescence (EL) and the device was prepared by vacuum thermal evaporation to obtain a yellow DC thin film with a peak wavelength of 575 nm Electroluminescence, thereby changing the luminescence color by doping. And a doped thin layer (Alq3: R6G) is inserted in different regions of the Alq3 light emitting layer. By using the difference between the emission wavelength and the undoped part (Alq3), the doped layer is used as a “detecting layer” Measurement and analysis, discusses the basic issues related to the light-emitting area, light-emitting mechanism, the impact of the interface on the light.