论文部分内容阅读
In order to get a sound casting of the alloy with a solidification range, the principle of directional solidification (DS) and the layer-by-layer solidification(LBLS) should be followed, especially in designing foundry process of steel casting. Using the principles, the reasons for the forming of the defects on the surface of the chain wheels teeth and groove and the forming of MT (magnetic particle testing) thin lines were analyzed. The results of the metallographic observation and the numerical simulation show that the low temperature gradient results in a wider mushy zone at the S/L interface that causes the defects and MT thin lines on the surface of the chain wheel casting. Based on the analysis, a new casting technology of the chain wheel was designed and used in the casting production successfully.