Spinel zinc ferrites ZnFe_2O)4,prepared by co-precipitation method using the zinc nitrate Zn(NO_3)_2·6H_2O and ferric nitrate Fe(NO_3)_3·2H_2O as the raw materials,were characterized by the thermo gravimetric analysis(TG)and differential scanning calorimeter(DSC),X-ray diffraction (XRD)and scanning electron microscope(SEM).The influence of synthesis conditions,such as Zn/Fe molar ratio,pH value,the sintering temperature and time,on the microstructures was detailedly in-vestigated.The relationships between the microstructures and the synthesis conditions were discussed.The results show that the pure spinel zinc ferrites ZnFe_2O_4 are formed when the Zn/Fe molar ratio is 1.05:2 at pH=8.5 or Zn/Fe molar ratio is 1:2 at Ph=9-10,and the precursors are sintered at 1100℃ for 4 h.Especially no other phases are observed when the Zn/Fe molar ratio is 1:2 at pH=10 and the precursor is sintered above 700 ℃for 4h.The higher sintering temperature and longer sintering time contribute to grain growth.
其他文献
Rigid polyurethane foams were fabricated with five kinds of liquefied sugarcane bagasse polyols(LBP).The foams derived from sugarcane bagasse were investigated by thermogra-vimetric analysis(TGA),and the thermal degradation data were analyzed using the Co
Structure characteristics of three kinds of ceramsite with different water absorption and the influence on microstructure of interfacial zone as well as performance of chloride permeabil-ity and frost resistance of combined aggregate concrete were investi
Formation and coexistence of tricalcium silicate(C_3S)and calcium sulphoaluminate (C_4 A 3(S))minerals in Portland cement clinker containing calcium sulphoaluminate were investigated. The f-CaO content,mineral composite and formation of mineral in the cli