铁水、钢水连续温度计

来源 :云南冶金 | 被引量 : 0次 | 上传用户:zhuxuan88
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
该温度计系由新日本制铁公司与旭硝子公司于1989年研制而成。传统温度计在钢水、铁水中只能测定1~3秒,因测温元件溶蚀于其中而不能再使用。此温度计采用熔点高达3060℃,耐热性超异的精细陶瓷材料硼化锆(ZrB_2)作外部保护管。热电偶为铂铑型(阴极:Pt8%, The thermometer by the Nippon Steel Corporation and Asahi Glass Company in 1989 developed from. The traditional thermometer in the molten steel, hot metal can only be measured 1 to 3 seconds, due to temperature measurement components dissolved in which can no longer be used. The thermometer uses a melting point of up to 3060 ℃, super-heat resistance of the fine ceramic material zirconium boride (ZrB_2) for external protection tube. Thermocouple type platinum and rhodium (cathode: Pt8%,
其他文献
This paper describes a new surgical techni-que for obtaining a better nasal contour in se-condary cleft lip nasal deformity. It involves re-moving of the curve
本文介绍了在轧辊上自己动手制作的电蚀凹形字符的电火花加工设备。投用三年来,达到投资少,上马快、运行可靠,适用于中小型轧钢厂。 This article describes the electro-er
本文主要分析新会计准则在供电企业中的影响,在此基础上探讨有效实施新会计准则的应对策略,以期对正在实施新会计准则及将要实施新会计准则的供电企业有所帮助。 This artic
尽管波音公司并未公布其777型喷气式飞机所使用的钛量,但从其10月中旬所发表的联合航空公司定购68架新型飞机的情况看,该公司正在加强向美国钛生产者的定货是肯定无疑的。
请下载后查看,本文暂不支持在线获取查看简介。 Please download to view, this article does not support online access to view profile.
日本日产汽车与日立粉末冶金公司开发出一种即使在1000℃的废气温度下也可使用的排气滑动构件。这种排气滑动构件是将钴基的硬质粒子分散在基体材料不锈钢内,进而为防止内部
孟尊荣今年39岁,热情直率。一眼看去,就是一位非常精明能干的人。1982年,朝阳区白家庄菜站的经营状况进入了最低谷。当时内外债务沉重,无钱进货,滞销的货却积压如山,几年来
在钻床上加工孔径大于50mm,厚度0.5~3mm的薄板工件比较困难,需将钻头磨成平角,才能加工。如用氧气切割,熔下来的铁碴附着在孔的周 In the drilling machine processing aper
据Stahl und Eisen No12,1990,P109报道,德国蒂森公司和振动测量仪表公司(SMS)合作,研制出一种早期识别连铸坯拉漏的智能自适应系统。在连铸操作发生变化,更换结晶器、改浇
目前线切割机断丝或换丝,都是手工拆丝,费工费时。如果在贮丝筒上,沿轴向铣一道浅槽,在断丝或换丝时,对于不能再利用的旧丝,可用剪刀沿槽将丝剪断,省工省时。 The current