冶山铁矿选矿厂1972年投产以来,选铜技术指标一直较低,1978年~1981年平均指标仅达到:铜精矿品位12.58%,铜实际回收率48.16%。生产实践表明,采用浮选柱作为铜钴混合浮选设备,不适应我厂浮选工艺的要求,于1981年8月以浮选机取代了浮选柱,铜的回收率有了较大幅度的提高,连续八个月的选铜的平均生产指标达到:铜精矿品位12.47%,铜实际回收率56.51%。 Since the ore dressing plant in Ye Shan was put into operation in 1972, the technical indicators for copper selection have been relatively low. The average indicator from 1978 to 1981 only reached 12.58% copper concentrate and 48.16% copper. Production practice shows that the use of flotation column as a copper-cobalt hybrid flotation device does not meet the requirements of our plant flotation process, in August 1981 to replace the flotation column flotation column, copper recovery rate has been more substantial The average production index of copper for eight consecutive months reached 12.47% for copper concentrates and 56.51% for copper.
其他文献
镇江焦化厂对煤焦油沥青进行热聚合改质与造粒,经过一年多时间的小试中试,已研制成符合要求的粒状沥青,并在1984年9月21~23日在镇江市由冶金部组织召开的鉴定会通过了鉴定。
冶炼厂采用铜精矿与金银矿料混炼联产的生产工艺后,收到了明显的经济效果。但由于联产过程,特别是电解精炼过程的能耗比例的确定较难,给定额管理带来困难,造成了管理上的混乱
马钢是一个综合性的钢铁联合企业,由于装备技术水平的不断提高和生产任务的不断加重,对设备的安全可靠性要求越来越高,50年代从苏联引进的计划预修制,已不能适应马钢生产发
传统的高炉炼铁法是一项复杂而庞大的生产工艺。从矿石到生铁要经过许多生产环节,原燃料经过反复加热、冷却和加工,大大提高了产品的成本和能耗。办了改变这一现状,炼铁工作
本文着重介绍了攀钢转炉炉龄试验及生产结果。由于确立了炼钢新渣系及适宜的冶炼工艺操作,创造出同类转炉炉龄711炉的先进水平。 This article focuses on the Panzhihua co
从高炉冶炼发展趋势出发,为提高副产品的应用价值及强化高炉生产过程、分析了煤气脱除 CO_2的意义和经济效果。按当前鞍钢高炉煤气组成,脱除 CO_2为30%,并以此加入高炉鼓风中
在采用成分稳定、理化性能较好的原燃料的前提下,十、十一高炉进行正分装大批重试验,提高了顺行压差,炉料透气性改善,炉况顺行变好;冶炼过程中选择合理的造渣制度;严格控制
一、生产情况 中国钨矿资源十分丰富,是世界上储量最大、产量最多的国家。现有40多个国营矿山和近200个矿点、42个重选厂和2个4000吨以上的精选厂在生产。生产能力逐步扩大,
本文研究了钯的加入量、烧结温度和烧结时间对钼的密度的影响。实验结果表明,钯的最适宜的加入量为0.5wt%左右。在这个最佳量下钼的最适宜的烧结温度为1150℃。利用实验数据计
机械工业部通用基础件局于一九八五年五月二十七日至二十九日在宁波粉末冶金厂主持召开了“氮基气氛在粉末冶金铁基零件烧结中应用”鉴定会。氮基烧结气氛作为粉末冶金铁基