针对退火炉内宽带钢跑偏的问题,分析了带钢跑偏的主要影响因素,介绍了连退机组炉内增设单辊纠偏装置技术的改造方案和项目的具体实施过程。
Aiming at the deviation of wide strip in annealing furnace, the main influencing factors of strip deviation are analyzed. The modification scheme of the single roller correcting device in continuous furnace and the concrete implementation of the project are introduced.