【摘 要】
:
从分析0.3~0.5mm不锈钢薄板钨极氩弧焊对接焊缝质量入手,提出了避免烧穿的新措施。除选定合适的焊接参数并保持其稳定外,关键是防止焊接过程熔池前间隙过大,或因失稳变形产生隆起和错边,这
论文部分内容阅读
从分析0.3~0.5mm不锈钢薄板钨极氩弧焊对接焊缝质量入手,提出了避免烧穿的新措施。除选定合适的焊接参数并保持其稳定外,关键是防止焊接过程熔池前间隙过大,或因失稳变形产生隆起和错边,这要求装配时起弧端尽可能无间隙,而在接缝末端有1.5~2mm的楔形间隙;焊接过程熔池前方始终保持小于0.05mm的间隙。
Based on the analysis of the quality of the butt weld of 0.3 ~ 0.5mm stainless steel TIG welding, a new measure to avoid burn through was put forward. In addition to select the appropriate welding parameters and maintain its stability, the key is to prevent the welding process before the weld pool gap is too large, or instability due to deformation of the raised and wrong edge, which requires the assembly of the arc as much as possible without gap, The end of the joint has a wedge-shaped gap of 1.5 ~ 2mm; welding process always keep the molten pool gap less than 0.05mm.
其他文献
国家经贸委在行业协会反倾销反补贴工作座谈会上提出,行业协会要明确职责,在反倾销、反补贴、保障措施工作中发挥积极作用。首先,行业协会要进一步认清自己的职责。行业协会作为
上海莱土公司生产的静脉注射人血免疫球蛋白拥有美国FDA许可的病毒灭活技术,使用方便,副作用小,能使病毒灭活,安全有效,因而在临床上广泛应用。现将我院1997年期间住院患者应用免
本文以生物组织切片偶合氧电极制成了组织切片过氧化氢电极。测试了电极的响应特性。在6.4×10~(-5)~1.2×10~(-3)mol/L 的过氧化氢浓度范围,该电极显示的电流变化与过氧化氢
用紫外分光光度法测定雏脑路通含量,在347±1nm 下,吸收度与浓度成直线关系,稀释倍数对含量无影响。
Ultraviolet spectrophotometry method for the determination of Naur
经营企业需在月度、季度和年度财务报告完成之后,必须及时、准确提供财务报告内部分析,以便于及时为各方投资者、企业负责人和管理人员提供可靠、有用的财务信息.本文从投资
研究了栗黄枯叶蛾核型多角体病毒(Trabala vishnou Nuclear PolyhedrosisVirus)的病毒粒子蛋白(Virion Protein),简称TV—NPV—VP,在不同pH值条件下于银胶中的表面增强拉曼光
目的研究替比夫定(Ld T)治疗妊娠中晚期乙型肝炎病毒(HBV)感染免疫耐受期高病毒血症孕妇的效果及停药后丙氨酸氨基转移酶(ALT)升高比例。方法选取该院2013年1月-2015年12月住
山东省枣庄市山亭区城头镇财政所积极帮助农民调整农业种植结构,邀请省农业专家对当地土壤、水惯进行测试,依据自然条件统一引进脱毒土豆良种,指导农民按标准化要求种植,确
一、案例背景新型农村合作医疗制度是保障和改善农村民生问题的一项重大社会政策,自2003年启动试点以来,已在全国各地快速发展并取得了巨大成就,但是在这个政策制定与调整的