Φ12~32 mm 20CrMo齿轮钢(/%:0.19~0.23C,0.48~0.58Mn,0.24~0.28Si,0.009~0.015P,0.003~0.012S,0.87~1.08Cr,0.17~0.18Mo,0.024~0.046Als)的生产流程为铁水脱硫-120 t顶底复吹转炉-LF-软吹-200 mm×200 mm方坯连铸-连轧工艺。结果表明,通过控制铁水[S]≤0.030%,BOF终点[C]≥0.08%,终点[P]≤0.012%,转炉出钢加0.6~1.0 kg/t铝块预脱氧控制L