论文部分内容阅读
(一) 企业中许多车间,通过修订与贯彻技术规程,生产面貌显著得到了改善。在那里,一些严重障碍生产而长期不得解决的问题解决了。例如:新沪钢铁厂冷铸车轮1955年连续5个月完不成质量指标的严重情况扭转了,裂纹、气孔、白口等废品第二季较第一季降低了62.5%;重庆一厂大平炉贯彻规程後,去年9月份合格率达到90.04%,开炉15个月以来首次完成了质量指标;华丰钢铁厂可锻铸件,改变了11个月未完
(A) Many workshops in the enterprise, through the revision and implementation of technical regulations, the production has significantly improved. There, some serious obstacles to the production of long-term problems can not be solved. For example: the cold steel wheels of the new Shanghai Iron and Steel Plant in 1955 for five consecutive months failed to complete the quality indicators of the serious situation reversed, cracks, pores, white mouth and other waste in the second quarter compared with the first quarter decreased 62.5%; Chongqing a factory Oven furnace After implementing the rules, the passing rate in September last year reached 90.04%, the first time since the furnace 15 months to complete the quality indicators; Huafeng steel plant malleable castings, changed 11 months unfinished