【摘 要】
:
鞍钢无缝钢管厂和科学院金属研究所等单位合作下,试验成功了穿不锈钢管用的钼基顶头,解决了长期未能解决的问题。过去这个厂生产1Cr18Ni9Ti不锈钢管时,一直使用20CrNi3钢的
论文部分内容阅读
鞍钢无缝钢管厂和科学院金属研究所等单位合作下,试验成功了穿不锈钢管用的钼基顶头,解决了长期未能解决的问题。过去这个厂生产1Cr18Ni9Ti不锈钢管时,一直使用20CrNi3钢的顶头进行穿孔。由于1Cr18Ni9Ti这种奥氏体不锈钢在高温时塑性低,变形抗力大,所以在使用20CrNi3顶头穿孔时,经常出现头部熔化、中部粘钢现象,使钢管造成严重的内折迭缺陷。为了减少这种缺陷,只好用一个
Anshan Iron and Steel Seamless Steel Tube Plant and the Institute of Metal Research and other units, the successful trial of wearing stainless steel tube molybdenum-based plug to solve the long-standing problems can not be solved. In the past when the factory produced 1Cr18Ni9Ti stainless steel tube, has been used 20CrNi3 steel piercing head. As 1Cr18Ni9Ti this austenitic stainless steel at low temperature plastic, deformation resistance, so the use of 20CrNi3 perforation, the head often melts, the middle of sticking phenomenon, the steel pipe caused serious defects in folding. In order to reduce this defect, had to use one
其他文献
(一)应用概况经过伟大的无产阶级文化大革命,广大工人群众掌握了马列主义、毛泽东思想武器,以阶级斗争为纲,遵照毛主席关于“打破洋框框,走自己工业发展道路”的教导,针对我
纵结构式船体在船台合拢时,由球缘扁钢组成的纵向支骨的对接焊是有些困难的,因球缘弯头部位内焊缝扣槽困难,而且施焊时焊工也难以看清楚,尤以在船体狭窄部位的质量更难保证
本文报导在0.15N盐酸介质中,用草酸作掩蔽剂,光度法直接测定锌基合金中稀土总量。方法简单,操作方便。
This paper reports the determination of the total amount of rare
在10%盐酸溶液中(V/V),钯(Ⅱ)与碘化钾形成红色络离子(PdI_4~(2-)),在波长408和480nm处有两个吸收峰。用抗坏血酸消除碘的颜色及合金中其他元素的干扰。方法简便、准确,用以
INTRODUCTION. Rare earth complexes with carboxylic acids have been investigated extensively, but little attention has been paid tothose with furan acid ligands
本文主要介绍上海锅炉厂为上海石油化工总厂建造的两个球形贮罐的焊接问题。文中包括材料可焊性试验、焊接材料选择、焊前准备及工夹胎具的使用、焊接过程、检验、返修及补焊
根据1980年4月召开的《化学通报》第二次全国编委会讨论意见,对本刊“主要栏目简介”和“征稿简则”作了适当修改。“进展与评述”栏的文稿,希望选题面要宽、读者面要广,适当
血清中氯的测定在临床检验上十分重要。常用的方法是二苯卡巴腙指示汞盐滴定法。这种方法不仅灵敏度低、需试样量较多,而且污染环境,对操作者有一定危害。近些年来,离子选择
地下水中微量酚的测定,可以不经蒸馏,用吐温—80乙醇液来抑制硫化物的干扰,在pH(?)10及氧化剂铁氰化钾存在的条件下,以4—氨基安替比林进行显色,加入聚乙烯醇作分散剂,以三
本文研究了氯仿萃取Pd—PY—TBF形成的三元络合物,以及络合物形成、萃取的最佳条件、反应机理和络合物的组成。一、仪器和试剂:东德VSU 2—P型分光光度计,江苏泰县无线电厂P