We adopted a new method, acid etching process, to fabricate the intrinsic Josephson junctions based on the Bi2Sr2CaCu2O8+x single crystals. By soaking the crystals into the dilute hydrochloric acid, we fabricated a junction stack successfully, and meantime made the surrounding area insulated. A certain concentration of hydrochloric acid was used to maintain the roughness of the modified layer. The cur-rent-voltage characteristic was achieved through the four terminal measurement. We could control the junctions’ number by changing the concentration and the soaking time. We also found that the thick-ness of the stack was equal to the average height of the insulation layer. Such a simple, convenient and controllable fabrication method with a high yield might widen the applications of the intrinsic Joseph-son junctions.
We adopted a new method, acid etching process, to fabricate the intrinsic Josephson junctions based on the Bi2Sr2CaCu2O8 + x single crystals. By soaking the crystals into the dilute hydrochloric acid, we fabricated a junction stack successfully, and meantime made the surrounding area insulated. A certain concentration of hydrochloric acid was used to maintain the roughness of the modified layer. The cur-rent-voltage characteristic was achieved through the four terminal measurement. We could control the junctions’ number by changing the concentration and the soaking time. found that the thick-ness of the stack was equal to the average height of the insulation layer. Such a simple, convenient and controllable fabrication method with a high yield might widen the applications of the intrinsic Joseph-son junctions.