Grain refinement of primary silicon in hypereutectic Al-Si alloys by different P-containing compound

来源 :中国铸造 | 被引量 : 0次 | 上传用户:li875
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
The grain refinement behavior of Si-3P, Si-25Mn-10P, and Al-10Si-2Fe-3P master alloys on hypereutectic Al-24Si alloy was studied. Microstructure analysis indicates that the P-containing compounds in the three master alloys are SiP, MnP, and AlP, respectively. The coarse flower-like primary silicon in the Al-24Si alloy transforms into smaller, well-distributed blocks with the addition of various master alloys. When pouring at 840 °C, the average grain size of the primary silicon refined by Si-25Mn-10P master alloy with a holding time of 30 min is about 18 μm, which is significantly smaller than those refined by Si-3P and Al-10Si-2Fe-3P master alloys. The grain size shows an increasing trend when the holding time is further prolonged. Higher holding temperature has a positive effect on the grain refinement of Si-25Mn-10P master alloy. The grain refinement mechanism of the three master alloys was also discussed.
其他文献
Many amorphous alloys have been developed to date, but the low plasticity has limited their application. To achieve an amorphous alloy with high plasticity, a s
To explore the corrosion properties of magnesium alloys, the chemical behavior of a high strength Mg97Zn1Y2-1wt.%SiC alloy in different corrosion environments wa
To refine the microstructure and improve the mechanical properties of AZ91D alloy by expendable pattern shell casting (EPSC), the mechanical vibration method wa