(Na0.5Bi0.5)TiO3相关论文
采用传统陶瓷工艺,研究了制备[(Na0.5Bi0.5)0.82(K0.5Bi0.5)10.18]1-xLaxTiO3(x=0.00,0.01,0.03,0.05,0.10)无铅压电陶瓷的工艺条......
以NaCl-KCl熔盐法制备了各向异性的Bi4Ti3O12粉体,研究了w(Bi2O3过量)对粉体的影响,优化了制备Bi4Ti3O12粉体的工艺参数。结果表明:w(Bi2......
采用传统固相法制备了0.6(Na0.5Bi0.5)TiO3-0.4(Bi0.1Sr0.9)TiO3陶瓷(即6BNT-4BST-9),研究了其相结构、铁电性能和储能特性;且利用复......