采用SrO和SrTiO3作为缓冲层,用激光分子束外延在Si(100)衬底上成功地外延生长出La1-xSrxMnO3(x=0.1,0.2,0.3)(LSMO)单晶薄膜.锐而......
采用SrO和SrTiO3作为缓冲层,用激光分子束外延在Si(100)衬底上成功地外延生长出La1-xSrxMnO3(x=0.1,0.2,0.3)(LSMO)单晶薄膜.锐而清晰的反射......