  This paper will focus on the most important stainless steel reference plants and the main innovative processes developed on stainless steel mills by Danieli Long Products Division.These technologies have been developed in order to fulfill the market growing demand of stainless steel mills combining-on the one hand-high plant productivity and efficiency with a superior quality of the finished products and-on the other hand-extreme process flexibility.The possibility to change process route according to the final application of the rolled steel grade and to simplify production planning is one of the most important keys to success that distinguishes stainless steel plants developed by Danieli.The last generation of on-line heat treatment technologies for stainless steels,presented on this paper,represents the core of Danieli know how on Stainless Steel production.
其他文献
For the purpose of reducing alloys additions and then its cost of conventionally combined Nb-V microalloyed Q460 grade steel plates for construction,a HSLA steel alloying design with only V-N microall
A steel composition substantially leaner than that of HSLA-100 steel was proposed in our previous work[1-5] to produce heavy plates with thickness of - 100 mm and mechanical properties equivalent to t
概述介绍了原油船货油舱(Cargo oil tanks)的腐蚀情况和主要防护措施,并对货油舱耐蚀钢发展历史、技术应用和国内外产品研制情况进行了阐述.结合原油船货油舱的腐蚀特点和国际海事协会(IMO)的耐蚀钢标准,阐述了当前原油船货油舱耐腐蚀防护措施以及发展原油船货油舱耐蚀钢的必然趋势,并表明为应对国内外造船市场对原油船用耐蚀钢板的潜在需求,发展原油船货油舱用耐蚀钢产品及其产业化应用技术已经刻不容缓
An ultra - high strength steel Q960E,produced by either thermomechanical control process with accelerated cooling plus tempering ( TMCP + AcC + T) or quenching plus tempering ( QT),was investigated wi
针对中厚板热轧时出现的边裂缺陷,研究了其形成原因及控制方法。结果表明,钢中[Al]、[N]控制不当,生成[AlN]析出造成晶界脆性,二冷水量冷却不均,结晶器振动偏摆量过大是边裂产生的主要原因。通过控制钢中[Al]、[N]的含量,合理降低连铸机二冷水量,优化结晶器参数等措施,减少了边裂缺陷的发生。
Steel plate suitable for high heat input welding were industrially produced by employing advanced steel-making technology and thermo-mechanically controlled processing and accelerated cooling technolo
Microstructures of 0.08% C-O.09Ti% and 0.08% C-O.025Nb% -0.09Ti% high strength heavy plates produced by TMCP are composed by banitic ferrite plates and martensite-austenite ( MA) constitutes locating
409L铁素体不锈钢冷轧板常规退火后为单一铁素体组织,而淬火一配分后为铁素体、马氏体和残余奥氏体的复相组织.常规退火板内有TiN、TiC和(Fe,Cr)23C6析出。而在淬火-配分板中,除TiN外,析出物总量显著减少,TiC大部分析出于马氏体中,此内还有(Fe,Cr)3C析出。淬火-配分板内残余奥氏体含量受淬火温度和配分时间的影响,因此,这两个工艺参数被优化以获得尽量多的残余奥氏体。在淬火-配分板
The oxidation kinetics of 443NT stainless steel in simulated combustion atmosphere and humid air at high temperature were studied by adopting thermal-gravimetric analysis ( TGA).The morphology,composi
Steel grade B445JIM was found to have more sticking possibility in hot rolling than that of grade SUS430.Oxide scale is a key factor affecting the sticking behaviour.In order to study the effect of wa