A new stepwise dissolution scheme, involving acids with different properties, enables the selective recovery of radiogenic and common Pb from a mineral, and ma
The infrared absorbance peaks at 2 852.4, 2 924.3, 2963.0 and 3 034.9 cm-1 have been observed in diamond films made by the direct current arc discharge plasma