论文部分内容阅读
最近,由于笔者着手试验页岩蒸养砖,为得到试验数据,把砖样送到“开县建筑质检站”.质检人员一看,说无法试压,原因是砖样不够,需30块.笔者听后感到茫然,因为我们没有批量生产,没有那么多的砖样.不得已问及试验程序及要求,并嘱其参照GB11945-89《蒸压灰砂砖》检测时,经解释,并带去标准全文,方同意可以用5块砖样先抗折后再行抗压,这样,尚有3块备用样品.
Recently, as the author started to test the shale steamed bricks, in order to obtain test data, the brick samples were sent to the “Qiang County Building Quality Inspection Station.” Quality inspection personnel saw it and said that it could not be pressure tested because the brick samples were not enough and required 30 pieces. The author was ashamed after listening because we didn’t have mass production, not so many brick samples. We had to ask about the test procedure and requirements, and consult them when referring to the GB11945-89 “autoclaved lime sand brick” test, explained and brought To go to the standard full text, the party agreed that it could use 5 bricks to bend first and then compress it. In this way, there are 3 spare samples.