论文部分内容阅读
Ceramic bond c BN composites with large pores were prepared by firing at 740 ℃ for 1 h using Na2O-Al2O3-B2O3-SiO2 glass and c BN abrasives( particles size 0.150 mm /0.124 mm) as main starting materials,c BN micro-particles( particles size 0. 014 mm) as th