论文部分内容阅读
Iron-based powder metallurgy material was prepared by warm compaction at 125℃ using a compacting pressure of 700 Mpa.Sintering temperature ranging from 1100℃ to 1300℃ and sintering time ranging from 40min to 80 min were used to study the effects of sinter