论文部分内容阅读
采用中频感应电炉在大气下熔炼Cu Cr中间合金 ,Cr以Cu 5 0Cr中间合金的形式加入 ,采用自配的专用覆盖剂 ,控制好熔炼工艺 ,最终获得Cr的质量分数为 4.0 %~ 5 .0 %的Cu Cr中间合金。