10Ni5CrMoV相关论文
The 10Ni5CrMoV steel examined was a 16 mm thick plate. Specimens measuring 12 mm × 12 mm × 120 mm were thermal......
采用系列温度冲击试验、动态撕裂(dynamic tear,DT)试验和落锤试验研究了10Ni5Cr Mo V钢错位同步双面双弧焊接接头的抗低温脆断性......
期刊
在1.6×10-3~1.2×103s-1的应变速率范围内,研究了应变速率对10Ni5CrMoV钢室温拉伸性能的影响。结果表明,应变速率对10Ni5CrMoV钢......