V150高抗挤毁套管相关论文
试验用Φ360 mm 27CrMnMoV钢(/%:0.27C,0.25Si,0.92Mn,1.06Cr,0.75Mo,0.009P,0.003S,0.088V)铸坯经穿孔和Φ340连轧机组热轧成Φ244.4......