Cr2O3 nanotubes with diameters of 80 nm and lengths of 550 nm were synthesized in a solvothermal reduction system at 180......
以乙二胺作为溶剂和碳源,用KBH4还原NiCl2得到的镍作为催化剂,于300℃制备碳纳米管.X-射线衍射(XRD)、透射电子显微镜(TEM)、选区......
以Fe3O4和葡萄糖碳化反应制备出的Fe3O4@C为载体,利用C层有助吸附Cu2+,将Cu2+吸附在Fe3O4@C表面,然后用乙二醇做还原剂成功制备出Fe3......