非均匀沉淀相关论文
采用非均匀沉淀法+酸腐蚀法制备形貌规则、窄尺寸分布、超细、单分散的γ-Al_(2)O_(3)纳米颗粒。首先,以硝酸铝、氨水为原腐蚀30 h......
通过分部固相法制备ZrW2O8粉体。以ZrW2O8、CuSO4·5H2O(分析纯)和无水Na2CO3(分析纯)为原料,采用非均匀沉淀法制备了Cu包覆ZrW2O8......
Three titanium-containing aluminum phosphate catalysts with a general formula Al0.77Ti0.23PO4 were prepared by the sol-g......
采用非均匀沉淀法包覆合成了LiNi0.9Co0.07Mn0.03O2锂离子正极材料。前驱体合成中各工艺条件与包覆材料的比表面积和电化学性能息息相......