The preparation of PET fiber modified polyethylene-wood composites (WPCs) was blended by double-screw extruder firstly and then heat-pressed to form panel materials with the thickness of 1 mm as the surface layer and the mass fraction of PET fiber was 0%, 3%, 6% and 9% respectively.