The AgSiO2 nanocomposite films loaded on silicon substrate surface were synthesized by pulsed laser deposition(PLD)at the incident energies of 140mJ/pulse for 60min at room temperature,with changing the Ag area ratio of the whole Ag/SiO2 target,we can get Ag-SiO2 nano-composite films with different Ag percentage.