The effects of the deformation in the non-recrystallization region of austenite and the cooling rate on the transformation behavior and microstructure of low-ca
<正>The alloy 5052 was welded by friction stir welding(FSW)and tungsten inert gas(TIG)welding.The effect of welding processes(FSW and TIG)on the fatigue propert
A novel 70Si30Al alloy was prepared by the spray forming process for electronic packaging materials. The effect of the ratio of atomization pressure to metal me