日本钢管公司继《特许公报》平5-72464号专利之后,又对所提出的铁基形状记忆合金作了进一步的改进,即是在原有的成分基础上添加了0.1Wt%~5.0Wt%的Mo,并且满足如下的成分条件:Ni+0.5Mn+0.4Co+0.06Cu+0.002N70.67(Cr+1.ZSi+Mo)-3。因为添加比能有效地提
Following Japanese Patent No. 5-72464, Japanese steel pipe company further improved the proposed iron-based shape memory alloy by adding 0.1Wt% to 5.0Wt on the basis of the original composition % Of Mo, and satisfies the following compositional conditions: Ni + 0.5Mn + 0.4Co + 0.06Cu + 0.002N70.67 (Cr + 1.ZSi + Mo) -3. Because adding than can effectively mention