论文部分内容阅读
在150℃的水热条件下可以合成SrO(?)SiO_2,当SrO和无定形SiO_2的摩尔比为1∶1时最有利于SrO·SiO_2形成,掺和3%的Na_2O有助于SrO·SiO_2晶体的生长并可提高SrO·SiO_2晶体结构发育的完善性.
Under the hydrothermal condition of 150 ℃, SrO (?) SiO_2 can be synthesized, which is most favorable for the formation of SrO · SiO_2 when the molar ratio of SrO to amorphous SiO_2 is 1: 1. Addition of 3% Na 2 O to SrO SiO 2 Crystal growth and improve the structural integrity of SrO · SiO 2 crystal structure.