In this study,Cu was added as the third additive to lower the sintering temperature of W-Ni-Fe alloy .By adding 2wt pct Cu, 2 dense 93W-3.5Ni-1.5Fe-2.0Cu tungsten alloy was obtained by hot-pressing at a low temperature of 1573K which is a process of liqui