在装配冷冲模时,凸凹模的间隙是否均匀一致将直接影响冲压件的质量。我厂过去在制造电机定子扇形片冲模时,当模具制造完后,检查间隙大体上一致,只有局部或大或小,但仍在合理的间隙(最大与最小间隙)之间。可是当试模时,局部出现小毛刺。为了解决冲模间隙的均匀性,可采用如下方法: 首先加工好的凸、凹模用汽油洗净,然后在凸模上涂一层均匀的漆片溶液(即漆片5%+酒精95%),待干后将凸模试插入凹模约4~8mm,以不能 Die assembly in the cold, punch and die gap is uniform will have a direct impact on the quality of stamping parts. In the past, when manufacturing the motor stator segment die, the inspection clearances were basically the same after the molds were manufactured, only partial or large but still within a reasonable clearance (the maximum and minimum clearances). However, when the test mode, a small local burr. In order to solve the uniformity of the die gap, the following method can be used: First, the processed convex and concave mold washed with gasoline, and then coated with a uniform coating solution on the punch (ie, 5% of the paint + 95% alcohol) , To be dry after the punch into the die about 4 ~ 8mm, can not
其他文献
(1)昼夜禁止居住地在二环路以外车辆所有人的电动三轮车,外地(含我市所辖的县市)牌号的轻便摩托车,普通二、三轮摩托车和车辆所有人登记注册的居住地在二环路以外的拖拉机、
本文就彩色不锈钢的国内外的情况、研制过程及应用范围进行了综合性的论述。 In this paper, the domestic and international situation of color stainless steel, the de
民间钓客之--Private fishermen县交通局退休干部林惠轩钟情垂钓,年逾七十有二的他,春钓溪边柳,夏钓池中莲,秋钓桂花香,冬钓瑞雪眠,常骑一辆老掉牙的自行车,肩背红布书包携饭
在5·12地震周年纪念和“六一”儿童节来临之际,为了能让灾区的孩子收到一份特殊的礼物,中国邮政、中国扶贫基金会联合开办“爱心包裹”行动。我觉得作为一名绿衣使者,有责任
北京时间7月6日,曼城以700万英镑的“白菜价”签下了阿森纳主力左边卫克利希。克利希效力阿森纳八年之久,作为“枪手”不败赛季的仅存硕果,他的离去意味着阿森纳失去了最后的
随着人们的精神和物质需求层次的提高,以人为本的设计产品相继问世,人性化设计在产品的创新与变革中越来越受欢迎,已经成为设计的主流。本文就是通过对人性化设计的相关特性
用3Cr2W8V材料制造的铝合金压铸模,依照常规淬火——回火处理。往往因粘模和磨损使用寿命不高,通过气体软氮化表面强化处理,可以有效地克服上述缺点,提高模具体使用寿命。本
用扭转变形研究Al—Mg—Si—RE合金高温变形对时效硬化行为的影响。结果表明:高温变形加速直接淬火后的时效析出过程;在固溶与形变温度相同时,变形温度愈高,时效硬化能力愈强
齿轮减速机是一种用途广泛的机械产品。由于市场需求量大,所以提出了制造质量好、速度快、经济效益高的要求。目前我国生产的齿轮减速机基本都是斜齿轮传动、嵌盖密封结构,
我校承接设计的真空泵泵体加工组合机床中,泵体的加工要求如图1所示;两轴承孔φ230的同轴度要求为0.05,两轴承孔的端平面为φ300,相距210~(+0.30),端面与孔的垂直度为0.04。