论文部分内容阅读
A two-step sintering method was used to prepare Al8.31Si1.91Mg3.78O20 (corundum solid solution)/Al4.8Si1.2O9.6 (mullite solid solution)/Mg2.0Al4.02Si4.98O18 (cordierite solid solution) multiphase material, for the purposes of making these three crystal st