原规格(16~25mm)热轧带钢不易卷取。通过改进精轧工艺的措施,在不影响带钢最终性能指标的情况下,提高带钢目标卷取温度,达到顺利卷取的目的。
The original size (16 ~ 25mm) hot-rolled strip is not easy to coiling. By improving the finishing rolling process, without affecting the final performance index of the strip, the target coiling temperature of the strip is increased so as to achieve the purpose of smooth coiling.