对加速器生产同位素56 Co 所用铁靶的制备工艺进行了研究。通过研究电沉积过程中影响 Fe靶层质量、电流效率的各种因素,确定了最佳工艺条件。制备出了质量厚度大于50 m g/cm 2,表面光亮、致密的 Fe 靶。
The preparation of iron target for 56C isotope production in accelerator was studied. By studying various factors that affect the quality and current efficiency of Fe target layer during the electrodeposition process, the optimum process conditions were determined. A Fe target with a surface thickness of more than 50 m g / cm 2, a bright surface and a dense surface was prepared.