论文部分内容阅读
铁山垄钨矿杨坑山选矿厂是一座日处理合格矿石625吨的钨选矿厂。原、次生矿泥量为出窿原矿的9%,含WO_30.31~0.45%,铜0.18~0.25%。钨金属量占原矿钨金属量13~15%,铜占18%。现在采用水泥刻槽摇
Tieshanchang Tungsten Mine Yangkengshan beneficiation plant is a daily processing qualified ore 625 tons of tungsten concentrator. The amount of primary and secondary sludge is 9% of the original ore, with WO_30.31 ~ 0.45% and copper 0.18 ~ 0.25%. Tungsten metal accounts for 13 ~ 15% of the original tungsten metal, copper accounted for 18%. Now using cement groove shaking