由于计量仪表质量欠佳,目前大多数高炉采用计算方法进行热能平衡.计算高炉煤气回收量前先要计算煤气的发生量,其计算方法有氮平衡法、碳平衡法等等.前者须入炉风量和煤气成分精确,后者也须各种原燃料的化学成分(包括挥发份的组成)与煤气成分等精确,计算起来都较为复杂.为计算简便,冶金部在1982年曾颁发的《钢铁企业能源平衡及能耗指标计算办法的暂行规定》 Due to the poor quality of measuring instruments, most blast furnaces use the calculation method for thermal energy balance. Calculate the amount of gas generated before calculating the amount of blast furnace gas recovery, which is calculated by nitrogen balance method, carbon balance method, etc. The former must be put into furnace Accurate air volume and gas composition, the latter also have to be a variety of raw fuel chemical composition (including volatile composition) and gas composition and other accurate, more complicated to calculate. For the calculation is simple, the Ministry of Metallurgical had issued in 1982, “Steel Enterprise energy balance and energy consumption indicators Interim Provisions ”
其他文献
把癌细胞特异性抗体作为抗癌药的载体,使抗癌药直接作用于癌细胞,这一疗法叫做癌的导弹疗法。本文对这一疗法的现状、存在的问题和发展趋势作一简述。从70年代后半叶,山口俊
在沉淀还原熔炼(OBП)粗锑过程中,有35%As进入返尘,这不仅增加了熔矿炉(PTП)的砷量,还使粗锑中砷的含量提高到3~3.5%。在提高含锑(30~35%)富砷(5~7%)精炼渣产率的情况下,精炼高砷
对于大型高炉,若长时间中心流过分发展,边沿流不足,必然会导致炉墙粘结,崩、滑料增加;而中心流比较发展,边沿流适当发展是理想的煤气分布。判断边沿气流是否发展,主要看十字
日本的一项专利(61-106733)提出的高纯锑制备法,是采用蒸馏法净化SbCl_3溶液,接着SbCl_3在氢气氛中还原。在盐酸水溶液中溶解Sb_2O_3时获得的氯化锑,用普通的蒸馏设备加热。
冶炼铸造铁时,在炉缸周壁上有大量石墨碳沉积使炉缸受侵蚀不多,因而能维护炉缸.当冶炼制钢铁,由于在[Si]
我国证券市场特殊的制度背景下存在着中期财务报告的自愿审计这一典型的研究课题。对自愿接受审计公司与未接受审计公司的经济后果进行研究发现,自愿接受中期审计的公司与未
硅热法炼镁,是因为可以直接采用分布广泛的白云石资源,能利用多种热源,设备和工艺流程较简单,建厂投资少,投产速度快,非常适合战争时期制镁的要求,所以同时在几个国家里迅速
干式煤气柜的开发、建造在我国尚属刚开始,特别是大型干式煤气柜,其制作安装技术要求相当高。本文仅就我院为湘钢设计的10×10~4m~(?)干式煤气柜作一浅析,简介该装置的优越性
本文较全面地介绍了粉末冶金技术及其在我国的现状。分析了当前我国粉末冶金工业存在的主要问题,并对加速我国粉末冶金的发展提出了建议。 This paper introduces the powde
金属粉末在成形和烧结过程中的尺寸变化是金属粉末的一项重要性能,与粉末零件的尺寸精度控制关系极大。 金属粉末在成形和烧结过程中的尺寸变化率按标准ISO4492—1978测定。