厚大钢铸件的铸孔方法

来源 :铸工 | 被引量 : 0次 | 上传用户:hzy11
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
我厂所铸的各种厚大铸钢件,单件重量最重达30吨以上,厚度最大至800公厘以上;这些厚大铸件的芯子在高温作用下,必须具有高度的耐热性,以达到容易清砂得到光洁铸件的目的。我厂除一些大型铸件用镁砂作面砂外,大部分用大罕砂造型,因此在一开始时,这些厚大铸件的铸孔,总是不易铸好,粘砂、渗铁较甚,给清理工作带来了很大困难,有的甚至因此而报废。为此,我们采取了以下的改进措施,并收到了效果。 I cast a variety of large castings of steel, the weight of a single up to 30 tons or more, the maximum thickness of 800 mm or more; the core of these thick castings at high temperatures, it must have a high degree of heat resistance , In order to achieve the purpose of easy clear sand get glossy castings. I plant in addition to some large castings with magnesia for the surface sand, most of the large sand shape, so in the beginning, these thick castings are always difficult to cast holes, sticky sand, iron infiltration more, The cleaning up brought great difficulty, and some even scrapped. To this end, we have taken the following improvement measures and have received results.
其他文献
请下载后查看,本文暂不支持在线获取查看简介。 Please download to view, this article does not support online access to view profile.
期刊
球墨铸铁是一种新的机械制造材料。由于具有优良的性能(高的降伏强度、抗张强度和疲劳强度,中等的延伸率和良好的耐磨性),可以用来代替可锻铸铁和一部分的铸钢。在最近几年
半液体金属模压是在摩擦压机上进行,它能直接利用热模锻所用的有飞边或无飞边锻模来压制毛胚。模压的工艺过程:用定量浇勺把熔化的金属注入敞开的模中,金属在模腔内停留相当
本文简要地论述了由安装误差求安装计算误差的一般公式。利用此一般公式能简便迅速地求出由于安装基面的误差及夹具原件的误差所产生的被加工表面的误差,并便于分析常用的一
我国机床型号是由金属切削机床实验科学研究所编制的,经第一机械工业部同意后自今年十一月起开始实施,为便于各方面的工作,故将我国机床型号与国外型号对照表刊出,供使用时参考。
在桥梁工程的施工建设中,施工裂缝是工程应当关注的问题。工程的质量问题在很大程度上是由于桥梁施工的裂缝引起的。因此,为保证桥梁施工和使用的安全,必须要对桥梁施工裂缝
转眼间,业余棋界规模最大、资格最老也最受人关注的晚报杯已经走过了十九个年头。从开始托关系我人承办到现在年年有多家晚报争办:从最初东拼西凑才拉到十几支队伍到现在年年
捷尔任斯基工厂用СЧ21-40和СЧ24-44灰铸铁铸造柴油机活塞、汽缸和汽缸套时,已不再用在个别情况下竟高达250公厘的冒口了(图1~3)。这是由于很好地运用了内浇口、集渣槽和
二、不锈钢钢析及钢卷用的炉子生产不锈钢钢板时基本上采用两种热处理方式: (一)在带淬火液的火焰炉内加热,然后钢板或钢带表面进行酸洗处理; (二)不锈钢在保护气体内光亮退
我們制造的鍵槽拉刀的規格和技术要求,請看圖1。材料用ХВГ鋼,經过鍛造、退火、机械加工后再热处理。在拉刀进行热处理的时候采用这样的工艺: 1.一次預热,溫度300~400℃(在