In this study,the low frequency electromagnetic casting (LFEC) technology was adopted to fabricate 2195 Al-Li alloy.The microstructure and solid solubility of as-cast 2195 alloys,as well as the second phase precipitation and tensile properties after aging,were investiagated and compared with the counterpart direct chill casting 2195 alloy.Our results indicate that LFEC can significantly improve the microstructure and metallurgical quality of as-cast alloy,and increase the number density ofθ\'(Al2Cu) and T1 (Al2CuLi) phases during aging treatment due to the enhanced solubilities of alloying elements.The tensile properties of 2195 aged alloy cast by LFEC were hence improved evidently.
其他文献
In this work,the influence of the Zener-Hollomon (Z) parameter on the microstructure and mechanical properties of copper subjected to friction stir welding (FSW) was investigated.Liquid N2 cooling was conducted to control the cooling rate after the FSW.Th
X80 pipeline steel plates were friction stir welded (FSW) under air,water,liquid CO2 + water,and liquid CO2 cooling conditions,producing defect-free welds.The microstructural evolution and mechanical properties of these FSW joints were studied.Coarse gran
AA6005A-T6 aluminum hollow extrusions were friction stir welded at a fixed high welding speed of 2000 mm/min and various rotation speeds.The results showed that the heat-affected zone (HAZ) retained the similar grain structure as the base material except
High electromagnetic shielding performance was achieved in the Mg-9Li-3Al-lZn alloy processed by accumulative roll bonding (ARB).The microstructure,electromagnetic interference shielding effectiveness (SE) in the frequency of 30-1500 MHz and mechanical pr
In order to study the effect of friction stir welding (FSW) on corrosion resistance of Al-Cu-Li alloy AA2099-T8,the microstructure and microhardness of FSW joints were characterized,and then,the corrosion behavior of the FSW joints was investigated by the
Dissimilar welded joints of reduced activation ferritic/martensitic (RAFM) steel and 316L austenitic stainless steel were prepared by friction stir welding with different butt joining modes and welding parameters.The weld quality of the joint was improved
Effects of long-term thermal exposure on γ\'particles evolution and impact toughness in the weld joint of Nimonic 263 (N263) superalloy were deeply studied at 750 ℃.Results showed that the precipitates in the weld metal were mainly composed of fine γ\
Friction stir processing (FSP),as a new kind of severe plastic deformation technique,can refine and homogenize the microstructure of metallic material.In this study,the effect of FSP on the microstructure and mechanical properties of pure Zr was investiga
Uniaxial tensile tests and stress-controlled low-cycle fatigue (LCF) and creep-fatigue interaction (CFI) tests of Inconel 625 alloy manufactured by selective laser melting (SLM) were performed at 815 ℃ in air environments.The microstructure was characteri
Direct laser metal deposition was used for preparing blocks of steel 12CrNi2 using four different laser powers under two different deposition environments including atmospheric environment and Ar-protected chamber.The results showed that microstructures a