The squeeze-casting method is utilized to synthesize ZL109/Al2O3·SiO2 particle reinforced composites with 5%,10%,20%,30%(volume fraction) Al2O3·SiO2 p
<正>The wrinkling has become the main defect in the thin-walled tube NC bending process. In the study, a dynamic explicit FE model for aluminum alloy thin-walle
<正>Al-Zn-Mg-Cu alloy is a favorable choice for aerospace applications requiring good combination of strength and toughness, which is greatly influenced by the
The electroless Ni-P-SiC composite coatings were prepared and the influence of vacuum heat treatment on its structure and properties was analyzed. The Ni-P-SiC
The high cycle fatigue properties and fracture behavior of 2124-T851 aluminum alloy were investigated roundly,including the fatigue crack growth rate,fracture t