【摘 要】
:
在全面分析已服役10年的HK40炉管损伤状况的基础上,研究了HK40炉管母材和焊接接头的蠕变裂纹扩展速率,评价了这2种不同部位抗蠕变裂纹扩展的能力。结果表明在长期正常的运行中,特别是服役后
论文部分内容阅读
在全面分析已服役10年的HK40炉管损伤状况的基础上,研究了HK40炉管母材和焊接接头的蠕变裂纹扩展速率,评价了这2种不同部位抗蠕变裂纹扩展的能力。结果表明在长期正常的运行中,特别是服役后期,下部炉管焊缝中的蠕变裂纹扩展比母材裂纹扩展快,微观组织损伤和焊缝中的应力集中是致使焊缝蠕变裂纹扩展较快的2个重要因素
Based on a comprehensive analysis of the damaged condition of HK40 furnace tube which has been in service for 10 years, the creep crack growth rate of base material and welded joint of HK40 furnace tube was studied, and the capability of creep crack propagation in these two different parts was evaluated. The results show that in the long-term normal operation, especially in the late stage of service, the creep crack growth in the lower tube weld is faster than that of the base metal. The damage of the microstructure and the stress concentration in the weld are the cause of the creep crack growth in the weld Faster 2 important factors
其他文献
材料的力学性能是指材料在外力作用下,表现出来的抵抗变形或破坏方面的特性。最典型的特性有弹性模量、屈服点、规定非比例伸长应力和抗拉强度等。规定非比例伸长应力又名“
针对常压塔顶冷换设备的腐蚀机理和特点,利用表面蒸发式空冷器独有的结构特点及钛材优良的抗腐蚀性能,研制开发出了钛复合板表面蒸发式空冷器。从而解决了常压塔顶冷换设备腐蚀
目的分别使用低剂量(1.1 GBq)和高剂量(3.7 GBq)131I对经甲状腺全切术后的中低危DTC患者进行治疗,比较不同剂量131I的清除甲状腺残余组织(简称清甲)结果、患者对治疗的反应有无差异。方法2014年10月至2015年6月,共140例(男37例,女103例,年龄18~75岁)患者入选。采用随机数字表法将经甲状腺全切术后的中低危DTC患者随机分配至低剂量组或高剂量组。(6±3)个月后评
渝麦14号(原名L-28)是四川农业大学农学院和重庆市农业科学院共同选育的小麦新品种。2011年5月通过重庆市农作物品种审定委员会审定(编号:渝审麦2011001)。该品种产量高,品质
青稞是藏区粮食生产的主要作物之一,介绍了青稞新品种北青9号的选育过程和特征特性及栽培管理技术。
Barley is one of the main crops for grain production in Tibetan ar
本文对视频信号采集的几种方法和相应的技术应用进行探讨。论述了利用8031和高速A/D转换实现视频信号采集;采用DMA Direct memoryaccess技术进行视频信号采集;利用高速比较器
推导了聚四氟乙烯波纹管和不锈钢加强圈的爆破应力与爆破压力算式,经算式计算和试件试验都表明,聚四氟乙烯波纹管的爆破系经向薄膜应力所致.阐述了爆破压力影响因素与提高爆
豫谷18是河南省安阳市农业科学院采用杂交方法从“豫谷1号×保282”中选育而成的夏谷新品种,该品种2010~2011年区域试验平均产量5 398.7kg/hm2,较对照冀谷19增产14.88%,居2010
唐花11号花生新品种是唐山市农业科学研究院利用航天育种技术,培育出的适合市场需求、符合外贸50-60出口标准的花生新品种。2010年12月获得河北省科学技术厅科学技术成果证书
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生、测量监控等方面人手,介绍了S226海滨大桥