提出了一种新的细化α+β型钛合金显微组织的氢处理工艺:在合金的氢化β转变点以下0—40K的温度范围对合金渗氢处理,空冷至室温,最......
A new process to refine the microstructure of α+βtvpe Ti alloys was developed by usinghydrogen as a temporary alloying......